A-A-50003D
Table II. End item visual defects.
Classification |
|||
Examination |
Defect |
Major |
Minor |
Material |
Any hole, tear, drop stitch, thin areas or mends Any slubs more than twice the thickness of normal yarn Any accumulation of slubs, clearly visible, causing non-uniform overall appearance Loose knitting Appearance of shade bars, birdseyes, miss-knit, tiger stripes, or dye streaks Color not comparable to standard sample Any spot or stain on outside more than 1/4 inch Rancid or bad odor |
101 102 103 104 105 |
201 202 203 |
Component |
Any component missing Any component part not as specified Any needle chew Any part badly pleated or caught or twisted in an unrelated row of stitching Any open seam Any bartack or tack omitted Any raw edge Any leg binding omitted |
106 107 108 109 110 111 |
204 205 |
Labeling |
Label omitted, incorrect, illegible or misplaced Not securely attached as specified, misplaced or stitching through printing. Bar code label not readable by scanner Human-readable interpretation (HRI) omitted or illegible Bar code label not visible on packaged item Any items not packaged in accordance with the contract or order |
112 |
206 207 208 209 210 |
5.3 End item testing and measurements. For the following test and dimensional examination, the sample unit shall be 12 drawers of one size, and the sample size shall be one sample unit for each size in the lot for lot sizes up to 12,000 pair of drawers, and two sample units for each size in the lot for the lot sizes of 12,001 or more.
5.3.1 Weight. Each sample unit shall be weighed unpacked for conformance to the minimum weight requirement as specified in Table I. The lot shall be rejected if any sample unit fails to meet the minimum weight requirement.